P1000 2020 1000-5 weld crack

Baumer8907

Baumer8907

Member
Apr 22, 2020
28
63
13
Ohio
Ownership

  1. 1000-5
I have a 1000-5 that has cracked at the weld. I wondered what people had the best luck with. I have thought about just replacing the y pipe. I was wondering if anyone else had taken off and re welded? Or if going to after market was the best? I wouldn’t mind a better tone, however I have outgrew the loud exhaust. Just wondering what would make the sense?



IMG 0372

IMG 0371

IMG 0370

IMG 0373

IMG 0374
 
JenElio

JenElio

NTC's NoMo Chupacabra Caliente!!....
Lifetime Member
Oct 31, 2019
82,548
716,423
113
Loxahatchee, florida
Ownership

  1. Other Brand

  2. 1000-5
I have a 1000-5 that has cracked at the weld. I wondered what people had the best luck with. I have thought about just replacing the y pipe. I was wondering if anyone else had taken off and re welded? Or if going to after market was the best? I wouldn’t mind a better tone, however I have outgrew the loud exhaust. Just wondering what would make the sense?



View attachment 448741

View attachment 448742

View attachment 448743

View attachment 448744

View attachment 448745
If you're not thinking of going aftermarket then I'd just weld/repair it and call it a day. The OEM is the quietest exhaust you'll find out there. If you're up for a little heat reduction, removing the CAT helps reduce heat a bit. You'll have the exhaust out already so you'll be halfway there. Quick and easy mod.

Good luck 👍
 
Baumer8907

Baumer8907

Member
Apr 22, 2020
28
63
13
Ohio
Ownership

  1. 1000-5
If I’m repairing, I feel like I should replace the y pipe vs welding. Where is the best place to order that from?
 
  • Like
Reactions: Backwoods and ChadD
Fatsquatch

Fatsquatch

Approved Member
Lifetime Member
Supporting Member
Jan 30, 2018
121,396
1,012,069
113
Hidden
If I’m repairing, I feel like I should replace the y pipe vs welding. Where is the best place to order that from?
Ronayers.com
Partzilla
Rockymountainatv
eBay … used or new
Local stealership

Personally if a fella can weld or has a friend that can….I’d weld it. Cost is next to nothing that way. But ultimately it is your decision
 
WagginTail

WagginTail

Well-Known Member
Lifetime Member
Club Contributor
Oct 13, 2020
1,652
6,061
113
SC
Ownership

  1. 1000-5
I have a 1000-5 that has cracked at the weld. I wondered what people had the best luck with. I have thought about just replacing the y pipe. I was wondering if anyone else had taken off and re welded? Or if going to after market was the best? I wouldn’t mind a better tone, however I have outgrew the loud exhaust. Just wondering what would make the sense?



View attachment 448741

View attachment 448742

View attachment 448743

View attachment 448744

View attachment 448745
Just weld it. No need to replace the y pipe. You could split a piece of pipe and put it over the crack and weld it, essentially making the pipe thicker in the area of the crack. That's what I would do if it was mine. Hope that makes sense.